Updated: 10 hours ago

How to Choose an Epoxy Marking Ink
The short answer
Pick an epoxy marking ink by how you apply it, how you can cure it, which A-A-56032 type the drawing calls for, and the color. Stamping or transfer marking points to ENTHONE M-Series, ACMI 6050 or ACMI 6600. Screen printing points to ENTHONE 50-Series, ACMI 6051 or ACMI 6601. If you have no oven, choose a two-part ink with a room-temperature cure; the one-part ACMI inks must be baked.
Four questions that pick the ink
How will you apply it? Rubber stamping and transfer marking need a thicker, paste-like ink. Screen printing needs an ink that flows through the mesh. Some inks also spray or roll.
How can you cure it? One-part epoxies need a bake. Two-part epoxies cure at room temperature over several days, or faster with heat.
Which A-A-56032 type? Type I is general marking, Type II is nonconductive (e.g. circuit boards) and Type III is outdoor exposure. With ENTHONE inks the type also depends on the catalyst and cure.
What color and finish? Check the drawing for a FED-STD-595 number, and whether it wants gloss or matte.
The epoxy inks we stock, side by side
Ink | Parts | Best for | Cure | A-A-56032 types | Colors |
|---|---|---|---|---|---|
Two (ink + catalyst, sold separately) | Hand stamping, machine and transfer marking; also screen, spray, roller | Room temperature or heat, set by the catalyst | I, II and III, depending on catalyst and cure (M0N black: I and III only) | 8, including inorganic black and cadmium red, orange and yellow | |
Two (ink + catalyst) | Screen printing; also spray, brush, roller | Set by the catalyst | A-A-56032, per the maker | Gloss and matte white, hi-hide white, clear, blues, black, nonconductive black | |
Two (kit) | Rubber stamping, offset printing | Room temperature (handle in 6–8 h) or force cure from 150°F | I, II and III | 11 EIA colors incl. silver | |
Two (kit) | Silk screen; also stamp or spray | Room temperature (handle in about 2 h) or force cure from 200°F | I, II and III | 11 EIA colors incl. jet black | |
One | Rubber stamping, offset printing | Bake: 300°F 30 min or 350°F 6 min | I, II and III | 11 colors incl. silver | |
One | Silk screen | Bake: 300°F 30 min or 350°F 6 min | I, II and III | 7 colors |
One-part ACMI inks have an essentially unlimited pot life because nothing cures until the bake. Two-part inks start curing once mixed: ACMI 6050 lasts about 4–5 hours, ACMI 6051 about 5–6 hours, and ENTHONE pot life runs from 1 to 24 hours depending on the catalyst.
Matching ink to the job
Hand-stamping part numbers on metal, no oven: a two-part stamping ink with a room-temperature cure: ENTHONE M-Series with an air-cure catalyst, or ACMI 6050.
Stamping in production with an oven: ACMI 6600 needs no mixing and stays usable all shift; bake to cure.
Screen-printing legends on circuit boards (Type II): a nonconductive ink: ENTHONE 50-770R or 50-771R, or ACMI 6051 or 6601. Avoid inks marked "not intended for electrical applications," such as ENTHONE M0N, 50-700R and 50-710R.
Type II with ENTHONE M-Series and no oven: use an air-cure catalyst rated for Type II, such as Catalyst 77 or B-13/28. Catalyst 20/A at room temperature does not meet Type II.
Parts that live outdoors (Type III): any of the inks rated for Type III, cured as the maker directs.
White legend on dark parts: ENTHONE 50-120R Hi-Hide White for screen printing, or M9N White for stamping.
Tips for good results
Clean the surface. Adhesion depends on a part free of oil, residue and particles.
Weigh, don't eyeball. Two-part inks are mixed by weight at the ratio on the technical sheet, and the ratio varies by color and catalyst.
Wait out the induction period. Let mixed ink stand before use: 15 minutes for ACMI 6051, 30 for ACMI 6050 and most ENTHONE catalysts, 60 for ENTHONE Catalysts 5 and 45.
Use the maker's thinner. ACMI says other thinners harm its epoxies.
Roll a thin film for stamping. Spread ink on a glass or metal plate with a brayer, then ink the stamp from that film.
Time the bake from part temperature. For baked inks, start the clock when the part reaches temperature.
Store it right. ACMI recommends refrigeration; one-part ACMI inks keep about 6 months, ENTHONE inks 3 years and catalysts 2.
FAQ
One-part or two-part: which is better?
Neither, it depends on your shop. One-part inks skip mixing and don't expire on the bench, but need an oven. Two-part inks can cure without heat but must be used within their pot life.
Do ENTHONE inks come with catalyst?
The catalyst is a separate component and is chosen for your cure process. Tell us how you'll cure and we'll recommend one.
Can I speed up a room-temperature cure?
Usually, yes. ACMI 6050 and 6051 list force-cure cycles from 150°F and 200°F, and ENTHONE catalysts can be heat cured.
Will the color match my FED-STD-595 chip exactly?
Not guaranteed. MacDermid gives FED-STD-595 numbers as approximate references, not certified matches.
Which spec do these inks meet?
All are made to A-A-56032, which replaced MIL-I-43553. See our A-A-56032 vs MIL-I-43553 guide and the spec cross-reference.
Still not sure?
Contact us with your part material, marking method, cure capability and the drawing callout.
Sources
MacDermid Alpha: ENTHONE M-Series inks (colors, deposition methods)
American Coding & Marking Ink: Government Specifications
Product technical sheets, as summarized on each product page
.png)